Products

Why your Nd:YAG failed to make enough energy

Short Description:

Nd:YAG (Neodimium Doped Yttrium Aluminum Garnet) has been and continue to be the most widely used laser crystal for solid-state lasers. Good fluorescence lifetime (twice more than that of Nd:YVO4) and thermal conductivity, as well as robust nature, make Nd:YAG crystal very suitable for high-power continuous wave, high-energy Q-switched and single mode operations.


Product Detail

Product Tags

It adheres on the tenet “Honest, industrious, enterprising, innovative” to develop new items frequently. It regards buyers, success as its very own success. Let us produce prosperous future hand in hand for Why your Nd:YAG failed to make enough energy, Together with our efforts, our products have won the trust of customers and been very salable both here and abroad.
It adheres on the tenet “Honest, industrious, enterprising, innovative” to develop new items frequently. It regards buyers, success as its very own success. Let us produce prosperous future hand in hand for China Crystal, high energy, Nd:YAG, Since always, we adhering to the “open and fair, share to get, the pursuit of excellence, and creation of value”values, adhere to the”integrity and efficient, trade-oriented, best way , best valve” business philosophy. Together with our all over the world have branches and partners to develop new business areas, maximum common values. We sincerely welcome and together we share in global resources, opening up new career together with the chapter.
Nd:YAG (Neodimium Doped Yttrium Aluminum Garnet) has been and continue to be the most widely used laser crystal for solid-state lasers. Good fluorescence lifetime (twice more than that of Nd:YVO4) and thermal conductivity, as well as robust nature, make Nd:YAG crystal very suitable for high-power continuous wave, high-energy Q-switched and single mode operations.

WISOPTIC provides Nd:YAG rods with the following features: different doping levels, high optical homogeneity, high processing accuracy, precise barrel grooving and wedge angle, various end cuts, various dielectric coatings, high damage threshold.

Contact us for the best solution for your application of Nd:YAG crystals.

WISOPTIC Capabilities – Nd:YAG

• Various options of Nd-doping ratio (0.1%~1.3at%)

• Various options of rods or slabs (flat, wedged, Brewster, grooved, etc)

• High optical homogeneity

• High processing accuracy

• High quality coating, high damage threshold

• Very competitive price, quick delivery

WISOPTIC Standard Specifications* - Nd:YAG

Standard Doping Ratio Nd%=0.1%~1.3at%
Orientation <111> or <100> or <110>
Orientation Tolerance +/-0.5°
Dimensions Diameter: 2~15 mm, Length: 3~220 mm
Dimension Tolerance Diameter (±0.05)×Length (±0.5) mm
Barrel Finish Ground with 400# grit, or polished
Flatness < λ/10 @ 632.8 nm
Surface Quality < 10/5 [S/D]
Parallelism < 10”
Perpendicularity ≤ 5′
Chamfer 0.15 ± 0.025mm @ 45°
TransmittedWavefront Distortion < λ/10 @ 632.8 nm
Clear Aperture > 90% central area
Extinction Ratio > 30 dB
Coating AR-Coating: R<0.10% @1064nm
Laser Damage Threshold > 800 MW/cm2 for 1064nm, 10ns, 10Hz (AR-coated)
* Products with special requirement upon request.

Nd-YAG-1
Nd-YAG-8
Nd-YAG-2

DOWNLOAD Technical Data – Nd-YAG


RoHS DOWNLOAD

Main Features - Nd:YAG

• High gain, low threshold, high efficiency

• Homogeneous distribution of Nd with subtle concentration gradient

• High thermal conductivity, high thermal shock resistance

• High homogeneity, low wavefront distortion

• High optical quality, low single pass loss (especially at 1064nm)

• Various modes of operation (CW, pulsed, Q-switched, mode locked)

Physical Properties – Nd:YAG

Chemical formula Y3-3xNd3xAl5O12 (x=Nd doping ratio)
Crystal structure Cubic
Lattice constants 12.01 Å
Density 4.55 g/cm3
Rupture stress 1.3~2.6×103 kg/cm2
Melting point 1970 °C
Mohs hardness 8~8.5
Thermal conductivity 14 W/(m·K) @20°C, 10.5 W/(m·K) @100°C
Thermal expansion coefficients 7.8×10-6 /K @<111>, 7.7×10-6 /K @<110>,
8.2×10-6 /K @<100>
Thermal shock resistance 790 W/m

Optical Properties – Nd:YAG

Laser transition

4F3/2 → 4I11/2 @ 1064 nm

Photon energy

1.86×10-19 J

Emission linewidth

4.5Å @ 1064 nm

Stimulated emission cross-section

2.7~8.8×10-19 /cm2 @ Nd%=1.0at%

Loss coefficients

0.003 /cm @ 1064 nm

Fluorescence lifetime

230 µs @ 1064 nm

Refractive index

1.818 @ 1064 nm

Pump wavelength

807.5 nm

Absorption band at pump wavelength

1 nm

Polarized emission

Unpolarized

Thermal birefringence

High